The parameters to be provided are as follows:
Compared with other galvanizing processes, the cleaning requirements for low carbon steel wire before galvanizing are low. However, under the current trend of increasing the quality level of galvanized layer, some pollutants brought into the plating tank are obviously harmful. Because cleaning galvanized coating wastes a lot of time and reduces the production, it is very important to properly clean and effectively rinse the substrate before electroplating.
When the zinc layer is seriously damaged and endangers the iron matrix, the zinc will produce electrochemical protection on the matrix, the standard potential of zinc is -0.76V and the standard potential of iron is -0.44V. When zinc and iron form microbatteries, the zinc will be dissolved as the anode, and the iron will be protected as the cathode. Obviously, the atmospheric corrosion resistance of hot dip galvanizing is better than that of electric galvanizing.
Customers in the order of wire mesh will often shop around, most customers are in comparison with manufacturers to give the product price, the company tells you, do not blindly compare the price. To standards, production technology, manufacturers and other factors lead to different prices.
With the improvement of people’s living standards, now many families are raising some small pets, these small pets need a stable nest, pet cage has become a more important choice of people, each pet habits and living habits will choose to adapt to the cage.
3, galvanized wire galvanized process
Cold galvanizing (galvanizing) is in the plating tank after the current unidirectional, so that the zinc gradually plated on the metal surface, slow production speed, uniform coating, thin thickness, usually as long as 3-15g, bright appearance, poor corrosion resistance, usually a few months will rust. Compared with hot dip galvanizing, the production cost of electric galvanizing is lower.
③ Galvanized iron wire shall not be damaged when it is tightened.Poor pretreatment before plating; Bath temperature is too low; Poor quality of additives or too many additives and organic impurities will cause poor bonding. The quality of additives also has an effect on coating foaming. Some additives react incompletely during synthesis and continue to polymerize during long-term storage or use. The additive tends to distort the crystal lattice and cause stress, causing the coating to bubble.